Tectron PPS Data Sheet

||Tectron PPS Data Sheet
Tectron PPS Data Sheet2017-01-23T10:02:26+00:00

Tectron PPS…

Tectron PPS 40% Glass-Filled Ryton PPS 40% Glass-Filled Ryton PPS
Mechanical ASTM Test Method Compression Molded PPS Compression Molded 40% GF PPS Injection Molded R-4 Units
Strength to Weight Ratio - - - - ksi
Specific Gravity @73 F D792 1.35 1.70 1.67 -
Tensile Strength @73 F, (ult)/(yld) D638 10,000 (ult) 13,000 (ult) 22,000 (ult) psi
Tensile Modulus of Elasticity @73 F D638 325,000 730,000 2,200,000 psi
Tensile Elongation at Break @73 F D638 5.0 2.0 1 %
Flexural Strength @73 F D790 18,000 23,000 29,500 psi
Flexural Modulus of Elasticity @73 F D790 370,000 1,000,000 2,100,000 psi
Shear Strength @73 F D732 - - 13,000 psi
Comprehensive Strength, (% Deformation) @73 F D695 18,000 (10) 24,000 (10) 26,000 (10) psi
Comprehensive Modulus of Elasticity @73 F D695 410,000 1,300,000 - psi
Hardness, Rockwell, Scale as noted @73 F D785 M93 (R125) M94 (R125) (R123) -
Hardness, Durometer, Shore D @73 F D2240 D85 D86 - -
Izod Impact, (Notched) @73 F D256 Type A 0.6 1.0 1.7 ft-lb/in of notch
Coefficient of Friction, (Dry vs Steel) Dynamic - 0.40 - - -
Limiting PV, (with 4 to 1 factor of safety applied) - - - - psi-ft/min
Thermal ASTM Test Method Compression Molded PPS Compression Molded 40% GF PPS Injection Molded R-4 Units
Coefficient of Linear Thermal Expansion @73 F E-831 (TMA) 2.8 E-05 2.5 E-05 - in/in/F
Heat Deflection Temperature @264 psi D648 250 490 500 F
Tg-Glass transition termperature, (Amorphous) D3418 - - - F
Melting Point, (VS=Vicat Softening Temp.) D3418 540 540 - F
Continuous Service Temperature in Air, (Max.) - 425 450 428 F
Thermal Conductivity - 2.00 2.10 2.10 BTU-in/hr-ft2-F
Electric ASTM Test Method Compression Molded PPS Compression Molded 40% GF PPS Injection Molded R-4 Units
Dielectric Strength, Short Term D149 540 385 450 Volts/mil
Volume Resistivity D257 4.5 E+16 - 1.0 E+16 ohm-cm
Dielectric Constant @10E6 Hz D150 3.0 - 3.8 -
Dissipation Factor @10E6 Hz D150 0.001 - 0.001 -
Flammability @3.1 mm unless noted UL94 V-0 V-0 V-0/5VA -
H2O ASTM Test Method Compression Molded PPS Compression Molded 40% GF PPS Injection Molded R-4 Units
Water Absorption, Immersion, 24 hours D570(7) 0.01 0.02 - % by weight
Water Absorption, Saturation D570(7) 0.03 0.03 0.05 % by weight