G-7 is a continuous filament glass cloth filler with silicone resin.  This composite material has good electrical properties under humid conditions, excellent heat and arc resistance, and is self-extinguishing. G-7 conforms to MIL-I-24768/17, MIL-P-997 and LP-509 military specs.

MechanicalASTM Test MethodValueUnits
Strength to Weight Ratio--ksi
Specific Gravity @73 FD7921.68-
Tensile Strength @73 F, (ult)/(yld)D63823,000psi
Tensile Modulus of Elasticity @73 FD638-psi
Tensile Elongation at Break @73 FD638-%
Flexural Strength @73 FD79023,000psi
Flexural Modulus of Elasticity @73 FD790140,000psi
Shear Strength @73 FD73217,000psi
Comprehensive Strength, (% Deformation) @73 FD69545,000 (10)psi
Comprehensive Modulus of Elasticity @73 FD695-psi
Hardness, Rockwell, Scale as noted @73 FD785M100-
Hardness, Durometer, Shore D @73 FD2240--
Izod Impact, (Notched) @73 FD256 Type A8.5ft-lb/in of notch
Coefficient of Friction, (Dry vs Steel) Dynamic---
Limiting PV, (with 4 to 1 factor of safety applied)--psi-ft/min
ThermalASTM Test MethodValueUnits
Coefficient of Linear Thermal Expansion @73 FE-831 (TMA)-in/in/F
Heat Deflection Temperature @264 psiD648-F
Tg-Glass transition termperature, (Amorphous)D3418-F
Melting Point, (VS=Vicat Softening Temp.)D3418-F
Continuous Service Temperature in Air, (Max.)-465F
Thermal Conductivity--BTU-in/hr-ft2-F
ElectricASTM Test MethodValueUnits
Dielectric Strength, Short TermD149350Volts/mil
Volume ResistivityD257-ohm-cm
Dielectric Constant @10E6 HzD1504.2-
Dissipation Factor @10E6 HzD1500.003-
Flammability @3.1 mm unless notedUL94V-0-
H2OASTM Test MethodValueUnits
Water Absorption, Immersion, 24 hoursD570(7)0.15% by weight
Water Absorption, SaturationD570(7)-% by weight