GPO-2 is a laminate formed from fiberglass reinforced with thermosetting polyester resins.

Mechanical ASTM Test Method Value Units
Strength to Weight Ratio - - ksi
Specific Gravity @73 F D792 1.80 -
Tensile Strength @73 F, (ult)/(yld) D638 9,000 psi
Tensile Modulus of Elasticity @73 F D638 - psi
Tensile Elongation at Break @73 F D638 - %
Flexural Strength @73 F D790 21,000 psi
Flexural Modulus of Elasticity @73 F D790 - psi
Shear Strength @73 F D732 - psi
Comprehensive Strength, (% Deformation) @73 F D695 30,000 psi
Comprehensive Modulus of Elasticity @73 F D695 - psi
Hardness, Rockwell, Scale as noted @73 F D785 M-105 -
Hardness, Durometer, Shore D @73 F D2240 - -
Izod Impact, (Notched) @73 F D256 Type A 8.2 ft-lb/in of notch
Coefficient of Friction, (Dry vs Steel) Dynamic - - -
Limiting PV, (with 4 to 1 factor of safety applied) - - psi-ft/min
Thermal ASTM Test Method Value Units
Coefficient of Linear Thermal Expansion @73 F E-831 (TMA) - in/in/F
Heat Deflection Temperature @264 psi D648 - F
Tg-Glass transition termperature, (Amorphous) D3418 - F
Melting Point, (VS=Vicat Softening Temp.) D3418 - F
Continuous Service Temperature in Air, (Max.) - 311 F
Thermal Conductivity - - BTU-in/hr-ft2-F
Electric ASTM Test Method Value Units
Dielectric Strength, Short Term D149 400 Volts/mil
Volume Resistivity D257 - ohm-cm
Dielectric Constant @10E6 Hz D150 4.95 -
Dissipation Factor @10E6 Hz D150 0.02 -
Flammability @3.1 mm unless noted UL94 V-0 -
H2O ASTM Test Method Value Units
Water Absorption, Immersion, 24 hours D570(7) 0.13 % by weight
Water Absorption, Saturation D570(7) - % by weight